Meaning
Fully lithiated state of a graphite anode where lithium ions occupy every available interlayer site. Formation of stage 1 lic6 occurs at the end of the charging cycle when the battery reaches its maximum capacity. This chemical configuration represents the highest energy density state of the carbon electrode.
Crystalline Transition
Graphite layers shift their alignment to accommodate the incoming metal atoms. The presence of stage 1 lic6 changes the color of the electrode from black or grey to a distinct gold or copper hue. This optical change is often used in laboratory settings to verify that the charging process was successful.
Thermodynamic Potential
Equilibrium between the solid phase and the liquid electrolyte determines the voltage of the cell. Maintaining stage 1 lic6 requires the potential to stay very close to zero volts versus lithium metal. If the potential drops below this level the lithium will plate on the surface instead of entering the graphite structure.
Structural Stability
Repeated expansion and contraction of the lattice puts mechanical stress on the binder and current collector. The transition to stage 1 lic6 involves a volume increase of approximately ten percent which can destabilize the interface between the electrode and the electrolyte. Continuous cycling into this state can lead to the fracturing of the graphite particles and a gradual loss of battery capacity over time.
This mechanical degradation is a primary reason for the eventual decline in the power delivery of the cell.