Meaning
Standardized procedure for determining the glass transition temperature of polymers and inorganic glasses using thermal analysis. By following the procedures defined in astm e1356, a laboratory can identify the precise moment when the internal molecular mobility of a polymer increases to the point where the material changes its physical state. It applies to materials that exhibit a distinct change in heat capacity during the transition from a glassy to a rubbery state.
The boundary for this method is reached when the transition is too broad or too weak to be distinguished from the baseline.
Testing Protocol
Data acquisition involves heating the specimen at a constant rate while monitoring the differential power. Results from astm e1356 identify the onset and midpoint temperatures of the transition.
Material Constraint
Application is limited to materials that are homogeneous and do not undergo simultaneous chemical reactions. If a sample decomposes or evaporates during the heating cycle, the accuracy of astm e1356 is compromised.
Standard Interpretation
Assigning the temperature requires linear extrapolation of the baseline before and after the transition. Final reports citing astm e1356 must specify the heating rate used because the glass transition is a kinetic event dependent on time.