Meaning
Mineral deposits composed of calcium sulfate dihydrate can accumulate on the internal surfaces of pipes and heat exchangers. This process, known as gypsum scaling, occurs when the local concentration of calcium and sulfate ions exceeds the thermodynamic solubility limit. Hydrometallurgical operations processing lithium and nickel ores are particularly susceptible to this issue due to their extensive use of sulfuric acid and lime.
The resulting crust restricts fluid flow and reduces heat transfer.
Deposition Mechanism
Heterogeneous nucleation on metallic or plastic surfaces initiates the growth of these mineral layers. Once the first crystals of gypsum scaling adhere to a surface, they provide a rough texture that accelerates further deposition. High temperatures in heat exchangers reduce the solubility of the mineral, making these zones highly vulnerable.
The crust thickens over time, creating a physical barrier to flow.
Equipment Failure
Uncontrolled crystal growth leads to severe damage. Clogged pipes reduce fluid throughput, while fouled heat exchangers require higher energy inputs to maintain process temperatures.
Control Measure
Refining facilities use a combination of chemical anti-scalants and physical cleaning cycles to manage this issue. Chemical inhibitors distort the crystal lattice to prevent adhesion, while high-pressure water jets remove existing deposits during scheduled maintenance shutdowns.