Meaning
Operation of introducing electrical energy into a battery cell at ambient temperatures below zero degrees Celsius requires specialized current and voltage profiles to accommodate sluggish electrochemical kinetics. This process, referred to as lithium-ion low temperature charge, represents a major challenge due to the high resistance of the cell and the increased risk of metallic lithium deposition on the graphite anode. It governs the charging speed of electric vehicle batteries in winter, and it must be terminated or modified if the cell temperature drops below specified survival limits, otherwise catastrophic failure may occur.
Charging Mechanism
Sluggish diffusion of lithium ions through the solid electrolyte interphase and inside the graphite particles leads to a large polarization of the anode during cold operation. Undergoing lithium-ion low temperature charge under these conditions causes the anode potential to drop below zero volts versus lithium reference, which is the thermodynamic threshold for lithium plating. This risk forces the use of much lower charging currents to prevent cell degradation.
Plating Prevention
Multi-step constant current profiles or pulse-charging strategies are used to adapt the current to the slow kinetics of the cell. These specialized protocols for lithium-ion low temperature charge aim to keep the anode potential above the plating limit while maximizing the energy stored. By adjusting the current based on state of charge and temperature, the system avoids the formation of dead lithium.
Thermal Control
Active heating systems integrated into battery packs represent a highly effective way to raise the cell temperature before initiating the process. Pre-heating the pack enables a safer and much faster lithium-ion low temperature charge by restoring the normal kinetic rates of the electrochemical reactions. This thermal management strategy reduces charging times and preserves the long-term safety of the battery system.