Quantifying Reversible Lithium Stripping Peaks through Differential Capacity Voltage Derivatives

Quantify reversible lithium stripping by integrating baseline-subtracted discharge dQ/dV peaks above 3.35V recorded immediately after low-temperature charge.

28.10.26 13 min

Inflection

An abrupt voltage shoulder at 3.38 volts disrupts the smooth profile of a commercial nickel-manganese-cobalt cell during early discharge. That localized signature indicates metallic lithium stripping from the negative electrode surface before graphite staging plateaus take over the terminal potential. When charging current forces the graphite surface potential below zero volts versus the lithium reference electrode, metallic lithium plates directly onto the composite matrix.

Reversing current dissolves that deposit back into the electrolyte as solvated ions before solid-state diffusion begins extracting intercalated ions from the carbon lattice.

Differentiating discharge capacity with respect to cell voltage converts that subtle shoulder into an isolated peak. Standard discharge curves obscure small phase transitions because the voltage drop across the stripping regime spans less than thirty millivolts. The derivative dQ/dV expands that narrow plateau into a distinct peak whose position, height, and area quantify the mass of metallic lithium returned to the liquid phase.

A stripping peak centered at 3.39 volts during a 0.5C discharge at five degrees Celsius accounts for twelve percent of the preceding charge capacity.

Phase transitions during discharge follow a strict thermodynamic sequence. The oxidation potential of metallic lithium sits lower than the delithiation potentials of graphite intercalation compounds. Staged graphite delithiation in the solid state occurs across distinct phases, starting with Stage 1 (LiC6 to LiC12) near eighty millivolts versus Li/Li+, followed by Stage 2 (LiC12 to LiC18) near one hundred twenty millivolts, with higher stages progressing above two hundred millivolts.

Metallic lithium dissolves first. Because this stripping reaction occurs at a lower negative-electrode potential, full-cell terminal voltage displays a temporarily elevated plateau early in discharge, ahead of the standard Stage 1 graphite delithiation plateau.

Thermodynamic Half-Cell Potentials and Full-Cell Discharge Signatures for Negative Electrode Reactions
Electrochemical Reaction Phase Half-Cell Potential vs Li/Li+ (V) Full-Cell Discharge Voltage Range (V) Differential Capacity Peak Character
Metallic Lithium Stripping -0.010 to +0.015 3.35 to 3.42 Sharp initial peak during early discharge
Graphite Stage 1 to Stage 2 (LiC6 to LiC12) +0.075 to +0.090 3.28 to 3.34 Broad intercalation peak following stripping
Graphite Stage 2 to Stage 3 (LiC12 to LiC18) +0.115 to +0.130 3.18 to 3.25 Distinct intermediate discharge shoulder
Graphite Dilute Stages (LiC18 to C) +0.190 to +0.230 2.95 to 3.10 Extended trailing baseline feature

Resolving this differential signal requires precise instrumentation. Standard production cyclers equipped with twelve-bit analog-to-digital converters introduce quantization steps that corrupt numerical differentiation, turning minor step changes into artificial derivative spikes that mask real electrochemical peaks. Clean derivative curves require twenty-four-bit voltage acquisition along with current control stability better than 0.01 percent of full scale.

Cell chemistry also plays a role: layered nickel-rich cathodes yield clear voltage separation, whereas lithium iron phosphate cathodes exhibit flat open-circuit voltage profiles that complicate early-discharge stripping identification.

Precision industrial machinery guides continuous metallic foil webs across rotating rollers inside a brightly lit battery manufacturing facility.

Phase Displacements during Graphite Delithiation

Terminal voltage during full-cell discharge reflects the difference between positive and negative electrode potentials, minus ohmic and polarization losses. As discharge begins, positive electrode potential declines steadily while negative electrode potential rises. As long as plated lithium remains on the anode, its potential stays pinned near zero volts versus Li/Li+, holding full-cell voltage above the normal graphite delithiation curve.

Once the surface deposit fully dissolves, the negative electrode transitions to the potential of the underlying lithiated graphite, causing a noticeable change in full-cell voltage slope.

Numerical differentiation registers this transition as a local maximum in dQ/dV. When negative potential shifts from zero volts to eighty millivolts, dV/dQ passes through an inflection point that forms a pronounced peak in the inverted dQ/dV domain. Lower temperatures widen this separation by increasing charge transfer resistance, driving overpotential higher and shifting the peak center.

A blue polymer film roll feeds upward through a precision mechanical guide unit mounted on an industrial workbench.

Foil

Current distribution across the negative current collector is rarely uniform. Variations in coating thickness, calender compression, and active material particle size create localized regions where lithium deposition starts early. Copper current collectors transfer charge through porous carbon coatings where ionic transport resistance in the liquid electrolyte exceeds solid-state electronic conductivity.

Under high charging currents, liquid-phase electrolyte potential drops steeply across the electrode thickness, hitting its most negative value at the separator interface.

Plating begins at the outer face of the graphite layer. Local overpotential relative to Li/Li+ turns negative near the separator first, even while active material adjacent to the copper foil remains incompletely lithiated. Once overpotential drops below zero, nucleation kinetics dictate deposit morphology.

High overpotentials promote mossy and dendritic structures with high specific surface areas, accelerating parasitic reactions with solvent molecules and additive salts.

  • Tortuosity gradients concentrate ionic flux in narrow pore throats, creating local overpotentials that cross the thermodynamic plating threshold before the bulk coating saturates.
  • Dead lithium detachment isolates metallic fragments from the conductive carbon matrix during discharge, severing electrical contact while trapping active lithium inside insulating passivation films.
  • Separator interface compression restricts volumetric expansion during rapid deposition, inducing micro-cracks across fragile solid electrolyte interphase layers.
  • Binder distribution anomalies cause local current crowding along the current collector boundary, triggering early dendrite growth along foil edges.
Solid electrolyte interphase consumption accelerates whenever dendritic growth expands the reactive metallic surface area exposed to solvent reduction.

During stripping, dissolution kinetics compete with mechanical detachment. The root of a dendritic stalk oxidizes rapidly because current density concentrates at high-curvature boundaries. If the neck dissolves before the rest of the structure reacts, the metallic tip disconnects from the graphite substrate.

That isolated fragment turns into inactive dead lithium, losing electrochemical contact with the circuit and vanishing from the differential capacity stripping peak. The area beneath the dQ/dV stripping peak reflects only reversible lithium stripping ~ the fraction of metal that kept electrical contact until fully oxidized.

The proportion of metallic lithium detached during stripping does not necessarily stay constant across successive cycles under fixed thermal conditions.

Extraction

Raw voltage time-series data requires mathematical conditioning before integration yields reliable capacity values. Differentiating unfiltered voltage data causes severe noise amplification, as numerical differentiation acts as a high-pass filter. Standard central-difference schemes turn millivolt-level measurement jitter into spurious dQ/dV spikes that obscure the true stripping signal.

Smoothing the voltage-capacity curve requires careful filtering. A Savitzky-Golay polynomial filter preserves peak height and area while stripping out high-frequency noise, provided window length and polynomial order match the physical width of the peak. A third-order polynomial spanning fifteen to twenty millivolts filters instrumentation noise without flattening the sharp inflection created by metallic phase dissolution.

A large cylindrical industrial capacitor sits beside a collection of small passive electronic components arranged on a dark worn workbench surface.

Where Do Voltage Plateaus Separate Stripping Signals?

Identifying integration boundaries requires separating the stripping peak from the underlying graphite delithiation baseline. Total discharge capacity in the initial voltage range combines metallic stripping with concurrent graphite deintercalation; baseline subtraction isolates the stripping component.

  1. Record discharge voltage and cumulative capacity at fixed intervals of one hundred milliseconds under continuous galvanostatic discharge.
  2. Apply a Savitzky-Golay filter using a third-order polynomial and a seventeen-point window to smooth raw voltage-capacity data without attenuating peak heights.
  3. Compute differential capacity dQ/dV by taking the central difference of smoothed capacity points divided by the voltage step.
  4. Identify the local minimum on the high-voltage side of the stripping peak to establish the upper integration boundary voltage.
  5. Construct a polynomial or spline baseline connecting the pre-peak inflection to the post-peak graphite Stage 1 baseline trough.
  6. Subtract baseline differential capacity from total differential capacity across the integration window.
  7. Integrate the baseline-subtracted dQ/dV curve with respect to voltage from lower to upper boundary to calculate reversible stripping capacity.

Spline baseline construction depends on precise boundary placement. The lower boundary sits at the start of discharge, right after the initial ohmic drop stabilizes. The upper boundary marks the valley where metallic stripping ends and pure graphite delithiation takes over the derivative slope.

Subtracting a cubic spline fitted between these two anchor points isolates the reversible stripping peak area.

Worked Parametric Sensitivity of Stripping Peak Extraction Under Varying Baseline Models
Discharge C-Rate Assumed Baseline Model Calculated Q_strip (mAh) Reversible Plating Ratio (%) Integration Error Margin (%)
0.2C Linear Tangent Fit 142.6 7.13 ±6.8
0.2C Cubic Hermite Spline 128.4 6.42 ±2.1
0.5C Linear Tangent Fit 198.2 9.91 ±8.4
0.5C Cubic Hermite Spline 181.5 9.07 ±2.7
1.0C Linear Tangent Fit 246.0 12.30 ±11.2
1.0C Cubic Hermite Spline 214.8 10.74 ±3.9
Test assumptions: 2.0 Ah nominal cylindrical cell tested at zero degrees Celsius following a 1.0C charge step. Reversible plating ratio calculated relative to nominal cell rating.

For a 2.0 Ah nominal cell charged at 1.0C at zero degrees Celsius and discharged at 0.5C, numerical differentiation of raw, unfiltered data yields erratic derivatives with peak variances exceeding thirty percent. Applying a third-order Savitzky-Golay filter across a seventeen-point window resolves a clear stripping peak centered at 3.385 volts. The choice of baseline fit alters the calculated yield: a linear baseline drawn between 3.320 volts and 3.440 volts gives 198.2 mAh of stripped lithium, while a cubic Hermite spline pegged to the graphite Stage 1 delithiation slope reduces that figure to 181.5 mAh.

The 16.7 mAh difference accounts for nine percent of the extracted value, illustrating how baseline definitions shape analytical results.

Evaluating Coulombic efficiency loss provides the second part of the calculation. Reversible stripping capacity Q_strip represents metallic lithium that re-oxidizes into the liquid electrolyte. Total plated lithium equals Q_strip plus irreversible lithium lost to dead metal formation and SEI growth.

While differential capacity derivatives measure Q_strip directly, determining irreversible plating requires tracking capacity fade across reference cycles conducted at twenty-five degrees Celsius.

Minor low-temperature differential capacity anomalies reflect either normal graphite phase shifts or metallic deposition phenomena.

Chamber

Thermal control during qualification testing governs the physical onset of metallic plating. Liquid diffusion coefficients in standard carbonate electrolytes drop by more than an order of magnitude between twenty-five degrees Celsius and minus ten degrees Celsius. Solid-state lithium diffusivity in graphite declines from approximately 10^-10 square centimeters per second at room temperature to less than 10^-12 square centimeters per second below freezing.

Under these constraints, incoming lithium ions accumulate at particle surfaces because insertion kinetics cannot keep pace with electrical charge transfer.

Industrial machinery processes conductive foil through precision metal rollers within a controlled environment while a large axial fan circulates air in the background.

Will Thermal Chambers Mask Subtle Overpotentials?

Forced-air environmental chambers create convective cooling patterns that mask internal cell heating. An unmonitored cell surface exposed to rapid airflow might read zero degrees Celsius on an external thermocouple while its core runs five to eight degrees warmer during high-rate charging. That core temperature rise accelerates local intercalation kinetics, suppressing plating inside while heavy deposition occurs along the cooler outer perimeter.

Reliable stripping detection requires environmental chambers with surface temperature variation verified within plus or minus 0.5 degrees Celsius across the entire can.

Baseline test profiles run without sufficient open-circuit rest periods obscure stripping peaks by convolving thermal relaxation transients into early discharge derivatives.

The rest period between charge completion and discharge determines whether a stripping peak appears in the derivative curve. When a fast-charged cell rests at open circuit, plated metallic lithium reacts spontaneously with underlying lithiated graphite via chemical re-intercalation. Because metallic lithium on the carbon surface has a higher chemical potential than vacant or partially filled graphite sites, lithium dissolves from the deposit and intercalates into the lattice without passing electrons through the external circuit.

This self-relaxation process gradually consumes the metallic deposit.

Stripping Peak Retention as a Function of Open-Circuit Rest Duration Prior to Discharge
Chamber Temperature (°C) Rest Time Before Discharge (min) Detected Q_strip Area (mAh) Chemical Intercalation Loss (%) Peak Potential Center (V)
-10 2 242.1 0.0 3.375
-10 15 218.4 9.8 3.378
-10 60 164.5 32.1 3.382
-10 240 52.3 78.4 3.390
0 2 181.5 0.0 3.385
0 15 132.8 26.8 3.389
0 60 41.2 77.3 3.398
0 240 0.0 100.0 None Detected

If an incoming inspection protocol specifies a two-hour rest period after low-temperature fast charging, chemical re-intercalation consumes the entire metallic deposit before discharge begins. The differential capacity curve then shows no stripping peak, which can lead to the false conclusion that no plating occurred during charge. Quantifying reversible stripping accurately requires keeping the rest interval under five minutes or tracking open-circuit voltage relaxation plateaus directly during rest.

Discharge rate during the detection cycle involves a clear trade-off. High discharge rates widen terminal voltage drops, pushing the stripping plateau deeper into noise and shifting the peak toward the graphite deintercalation regime. Lower discharge rates preserve thermodynamic separation between stripping and delithiation, but extremely low rates extend test duration enough for chemical re-intercalation to consume metallic lithium during measurement.

A discharge rate of 0.2C to 0.5C offers the most practical compromise for commercial cells.

Plating detection is most reliable when discharge begins immediately after charging stops, before surface deposits chemically relax into the host matrix.

White polymer separator film routes through polished steel guide rollers inside a high precision lithium ion battery manufacturing machine.

Liability

Safety documentation for transport clearance relies on design verification records showing that cells remain stable under electrical abuse. Under UN 38.3 Test T.7, overcharge testing evaluates whether secondary batteries survive prolonged charging without fire or disassembly. While the standard sets clear pass/fail criteria based on immediate thermal runaway, it leaves the accumulation of dead metallic lithium from prior low-temperature cycles unaddressed.

Repeated unmonitored plating turns a compliant cell into a latent transport hazard. Metallic lithium deposits compromise the safety profile established by the original UN 38.3 test summary. Over operational cycles, dendritic structures can penetrate separator pores, forming localized micro-shorts that elevate self-discharge.

This invalidates initial transport declarations when shipping cells at high states of charge. Under European Agreement concerning the International Carriage of Dangerous Goods by Road (ADR) Special Provision 376, cells classed as damaged or defective face carriage prohibitions or require specialized containment packaging that increases freight costs tenfold.

Dendrite proliferation inside porous separators voids standard shipping declarations by reclassifying certified cells as defective goods under transport rules.

Commercial warranty terms routinely exclude cell degradation resulting from out-of-spec charging. Product datasheets define operating temperature envelopes and maximum allowable charging currents across specific temperature bands. A typical specification permits 1.0C charging at twenty-five degrees Celsius, restricts charging to 0.2C between zero and ten degrees Celsius, and bans charging entirely below zero degrees Celsius.

When field failures occur, differential capacity voltage derivatives extracted from battery management system non-volatile memory logs provide forensic proof of out-of-spec fast charging.

Extracting stripping peaks from warranty return cells provides definitive evidence during claim evaluations. If an energy storage system or vehicle fleet operates under charging profiles that drive graphite overpotential negative, the resulting dQ/dV stripping signature confirms that operating boundaries were violated. Contractual disputes turn directly on baseline integration thresholds used to calculate stripped capacity; buyers without internal metrology to evaluate baseline assumptions risk forfeiting warranty recourse.

Supply agreements incorporating quantitative degradation thresholds protect buyers only when verification methods specify derivative filtering parameters and baseline subtraction equations directly in the contract. Standard warranty clauses that merely guarantee capacity retention after a fixed cycle count allow grading conditions that mask plating damage behind room-temperature baseline cycles. Specifying dQ/dV stripping peak limits inside the cell purchase agreement establishes an enforceable metric for batch acceptance and warranty enforcement.

Section 7.3 of IEC 62660-2 mandates that safety evaluations confirm cell integrity after repeated cycling, and incorporating differential capacity stripping quantification into incoming quality agreements provides clear technical proof that delivered production lots comply with specified thermal operating boundaries.

Nomenclature

Savitzky Golay Filter

Meaning ~ Digital signal smoothing algorithms based on local polynomial regression describe the mathematical techniques used to reduce noise in electrochemical measurement data without distorting the underlying signal.

Stripping Peak

Meaning ~ Electrochemical signal observed during voltammetry measurements indicates the dissolution of metallic lithium previously plated onto the anode surface.

Tortuosity Gradient

Meaning ~ Microstructural configurations in battery electrodes that vary through the thickness of the active material layer control the balance between energy and power density.

Negative Electrode Overpotential

Meaning ~ Electrochemical polarization metrics measure the deviation of the anode potential from its equilibrium value during the passage of electrical current through a lithium-ion cell.

Dead Lithium

Meaning ~ Electrochemically inactive metal that has lost electrical contact with the anode collector reduces the usable capacity and lifetime of lithium ion batteries.

Baseline Subtraction

Meaning ~ Signal processing that isolates the true electrochemical response of a battery by removing background noise or steady-state offsets enables precise analysis of transient events.

Lithium Stripping

Meaning ~ Electroplating degradation involves the metallic deposit formation occurring on an anode surface during the discharge cycle of a rechargeable electrochemical cell.

Reversible Stripping

Meaning ~ Electrochemical dissolution reaction removes deposited metallic lithium from a substrate back into electrolyte ions during cell discharge without forming dead metal or structural moss.

Dq Dv Derivative

Meaning ~ Mathematical differential curves plotted against cell potential translate flat charge plateaus into distinct voltage peaks corresponding to specific phase transitions.

Copper Current Collector

Meaning ~ Metallic foil supplying electron conduction pathways inside a lithium-ion battery electrode structure requires a copper current collector to transport electrons from active material particles toward external terminals during discharge cycles.

Current Collector

Meaning ~ Electrically conductive substrate within an electrochemical cell provides a continuous low-resistance transport path for electrons between external terminals and active electrode materials.

Open Circuit Voltage

Meaning ~ The difference in electrical potential between the positive and negative terminals of a battery cell when no current flows.

What the firm knows, published