Meaning
An electrochemical parameter measures the difference between the initial charge capacity and the subsequent discharge capacity during the first cycle. High first cycle capacity loss occurs because of the formation of protective passivation layers on the electrode surfaces. This initial consumption of lithium is permanent and represents a major factor in cell design calculations.
The value is calculated by subtracting the first discharge capacity from the first charge capacity and is typically expressed as a percentage of the initial charge capacity.
Irreversible Consumption
Electrochemical reduction of the electrolyte solvent molecules on the anode surface builds the solid electrolyte interphase. This formation phase of first cycle capacity loss immobilizes active lithium ions from the cathode material. The reaction cannot be reversed during subsequent discharge steps because the lithium becomes chemically bound in the passivation layer.
Measurement Protocol
Constant-current cycling runs determine the initial coulombic efficiency of the assembled cell. Determining first cycle capacity loss requires subtracting the first discharge capacity from the first charge capacity. Testers execute this procedure at low currents to ensure complete passivation layer growth.
Anode Contribution
High surface area carbons or silicon alloys demand more active lithium to establish stable surface passivation. Choosing materials with lower surface area reduces first cycle capacity loss. Lower loss translates directly into higher energy density because less excess cathode material is needed to compensate for the initial deficit.