First Cycle Efficiency Deficits in Hard Carbon Anodes
Hard carbon initial coulombic efficiency deficits of 15 to 35 percent require aggressive cathode over-coating, pre-sodiation, or precise low-rate formation tuning.

Hard carbon initial coulombic efficiency deficits of 15 to 35 percent require aggressive cathode over-coating, pre-sodiation, or precise low-rate formation tuning.