Meaning
Mechanical shearing of metallic foils often results in a permanent protrusion of material at the cut edge. Roll-over burr height measures the vertical distance from the foil surface to the peak of the deformed metal. This dimension is a primary quality metric for slitting and blanking operations in battery cell assembly.
The measurement is confined to the physical distortion caused by the downward force of the cutting tool.
Plastic Deformation
Pressure from the blade exceeds the yield strength of the aluminum or copper current collector. This causes the metal to flow into the clearance gap before it actually fractures.
Separator Integrity
Large protrusions can create localized pressure points against the polymer membrane. In extreme cases, the metal peak penetrates the separator and causes an internal short circuit that may lead to thermal runaway. Safety standards for cell production typically limit this height to less than half the thickness of the separator.
Inspection Standard
Automated vision systems or contact profilometers verify the quality of the cut edges in real time. Samples are taken at regular intervals to ensure that the roll-over burr height does not exceed the engineering limit. Values trending upward indicate that the slitting knives are becoming dull and require maintenance.