Meaning
Parasitic surface structural transformation alters active cathode material interfaces from electrochemically active layered geometries to inactive cubic structures. Formation of a surface rock-salt phase occurs when transition metals lose oxygen and migrate into lithium layer sites during high-voltage operation or high-temperature storage. The resulting nickel oxide-like disordered structure lacks open pathways for lithium ion transport.
This degraded surface layer isolates active material cores from efficient electrochemical participation.
Degradation Pathway
High operating potentials and elevated temperatures strip oxygen atoms from the outer crystal lattice of cathode particles. During this structural breakdown, surface rock-salt phase formation accelerates through continuous contact with acidic species in the liquid electrolyte. Transition metal cations, particularly divalent nickel, easily occupy vacant lithium sites in the damaged outer atomic layers.
This cation rearrangement destroys the two-dimensional pathways necessary for rapid lithium intercalation.
Interfacial Resistance
Electrochemically inactive surface layers impede charge transfer reactions across the electrode-electrolyte interface. As the surface rock-salt phase thickens, cell internal resistance increases substantially, causing voltage polarization and power output loss. Higher resistance leads to localized thermal buildup during fast charging.
Layer Boundary
Surface transformation remains confined to the outermost atomic layers under controlled operational conditions. Typical rock-salt layer thickness spans from two to ten nanometers on particle surfaces. Beyond this thin interfacial shell, the surface rock-salt phase remains absent within the bulk structural framework.