Meaning
Structural and electrical deterioration of internal current collector joint interfaces increases electrical resistance and thermal stress within lithium-ion cell packages. Located at the joint connecting internal electrode foil stacks to external cell terminals, tab junction degradation arises from ultrasonic welding fatigue, intermetallic compound growth, thermal cycling, and localized corrosion. Mechanical vibrations and differential thermal expansion loosen welded interfaces, reducing cross-sectional conductive area.
Higher contact resistance generates localized ohmic heating during high-current operation, accelerating capacity fade and cell failure risks.
Failure Mechanism
Ultrasonic welds between aluminum or copper foils and nickel-plated copper tabs experience cyclic mechanical strain during pack operation. Micro-cracking along weld nuggets reduces current distribution uniformity, concentrating electrical current through remaining sound joints. Over time, tab junction degradation elevates localized joint temperatures above eighty degrees Celsius, triggering electrolyte breakdown and localized gas formation near cell seals.
Electrical Resistance
Internal resistance growth across degraded tab joints causes voltage drops under heavy discharge loads. Battery management systems detect this resistance increase as anomalous cell voltage imbalance, limiting available pack output power.
Quality Control
Non-destructive testing protocols using micro-ohm resistance meters and acoustic microscopy verify weld integrity before electrolyte filling. Strict mechanical pull tests and thermal shock protocols prevent tab junction degradation from compromising field reliability in electric vehicle battery packs.