Meaning
Localised dissolution and metallurgical degradation of an aluminium structural core substrate occur when excessive molten silicon-bearing braze filler penetrates and consumes the underlying base metal. The process operates during controlled atmosphere or vacuum brazing cycles of battery cooling plates when thermal holding times exceed operational windows. Liquid aluminium-silicon filler dissolves adjacent core metal to satisfy phase diagram equilibrium concentrations, thinning structural walls and compromising channel integrity.
Residual wall thickness drops below design margins, reducing internal burst pressure limits and increasing susceptibility to cyclic fatigue failure. The classification applies to liquid metal dissolution phenomena occurring during the thermal joining cycle, excluding electrochemical galvanic corrosion, erosive coolant flow wear and ambient mechanical rubbing.
Dissolution Kinetics
Interfacial dissolution initiates the instant clad filler transitions into a liquid phase above its eutectic temperature. Molten silicon atoms diffuse across the solid-liquid interface into base metal grains, lowering the melting point of adjacent core boundaries. Base aluminium dissolves outward into the liquid pool until the liquid reaches saturation equilibrium at the furnace holding temperature.
Higher peak temperatures widen the solubility limit of aluminium inside the melt, accelerating the consumption rate of the solid substrate. Extended exposure at peak temperatures allows dissolution to continue until the core metal suffers severe localized cross-sectional thinning.
Boundary Penetration
Preferential attack proceeds along core grain boundaries where elevated energy states and interfacial segregation accelerate liquid penetration. Liquid filler infiltrates deep between structural grains, enveloping individual crystals and detaching them from the bulk core matrix. This intergranular mechanism turns cohesive load-bearing material into a fragile network of brittle silicon-rich phases.
Fine recrystallised grain structures present dense boundary networks, multiplying pathways for liquid penetration compared to coarse-grained tempers. Residual cold-working stress acts as an additional kinetic driver, pulling liquid braze metal inward along slip bands and shear zones.
Structural Impact
Thinning of coolant channel walls undermines the structural pressure boundary separating battery pack electronics from conductive glycol solutions. Internal cooling plates subject to core erosion suffer premature burst failures at pressures far below typical proof specifications. Localized structural erosion acts as an acute stress riser under cyclic road vibration and dynamic thermal expansion loads.
Dissolved manganese from the core shifts the local fillet chemistry, degrading the galvanic balance between the remaining core metal and adjacent joints. Preventing core erosion requires restricting peak furnace cycle times and limiting clad thickness percentages to absolute minimum requirements.