Meaning
A structural and chemical breakdown of high nickel cathodes involves the loss of active material and the formation of resistive layers. This NMC811 cathode degradation occurs as the nickel rich lattice becomes unstable at high states of charge. It limits the cycle life of high energy density cells and establishes the maximum voltage threshold for long term use.
Microscale Change
Particle cracking and surface phase transitions reduce the surface area available for lithium ion exchange within the cathode. During NMC811 cathode degradation, the transition from a layered to a rock salt structure creates a barrier that slows down the reaction significantly. This mechanical fatigue results from the repeated expansion and contraction of the particles as lithium ions move in and out.
Microscopic fractures allow electrolyte to penetrate the core of the particles and cause further damage.
Electrolyte Interaction
Highly reactive nickel ions at the surface catalyze the decomposition of the surrounding fluid. The products of NMC811 cathode degradation form a thick film that increases the internal impedance of the battery. Additives are often used to coat the cathode and protect it from these destructive cycles.
Performance Impact
Capacity loss and power fading are the primary signs that the cathode is failing. As NMC811 cathode degradation progresses, the ability of the cell to deliver high current diminishes. Balancing the energy density benefits against these wear factors is the primary challenge for pack designers.