Meaning
Separation of the electrical connection between the current collector and the active material within a lithium ion battery cell constitutes this structural defect. Tab detachment failure mode occurs when mechanical stress or poor adhesion at the bond interface causes the current conducting foil to pull away from the internal electrode stack. This loss of connectivity interrupts the electron flow path, which increases the internal resistance of the cell and renders the device incapable of sustaining a charge or discharging energy.
Physical Mechanism
Cyclic expansion and contraction of the electrode layers during battery operation generate shear forces at the welding point. Frequent thermal changes aggravate these stresses, especially if the ultrasonic weld or laser bond between the tab and the foil lacks sufficient metallurgical fusion. Eventually, the weakened joint breaks under repeated displacement, permanently isolating the active electrode area from the external terminals.
Detection Protocol
Voltage drops during routine cell formation or charge cycles signal that an internal connection issue exists. Production lines verify the integrity of these joints through non-destructive testing such as milliohm resistance measurements taken at the terminal posts. An unexpectedly high resistance value relative to a control group indicates that the tab interface has failed or is in the process of fracturing.
Performance Consequence
Total capacity loss follows whenever the conductive link between the anode or cathode and the tab ceases to function. Batteries affected by this condition suffer from degraded power density, as the remaining intact area must carry the total current load alone. Localized heating often occurs at the point of detachment, potentially causing thermal runaway if the circuit path remains unstable during high current discharge events.