Meaning
Compressive forces are used in the deep drawing process to thin the vertical surfaces of a metal container while extending its length. Wall ironing pressure occurs as the cup is forced through a die with a clearance smaller than the original material thickness. This step is fundamental in producing the lightweight yet strong cases used for cylindrical batteries.
It ensures a uniform outer diameter and a smooth surface finish.
Friction Coefficient
Managing the heat and surface contact between the workpiece and the die is necessary to prevent galling. Proper wall ironing pressure is maintained through the use of high performance oils that form a protective film. If the force is too high, the material may snap or develop microscopic tears.
Constant monitoring of the press load helps maintain production quality.
Shell Geometry
The final height of the battery shell depends directly on the amount of material displaced during the ironing stages. Sufficient wall ironing pressure creates a work hardened surface that improves the structural rigidity of the shell. This hardness allows the container to withstand the crimping forces during the final sealing process.
Dimensional accuracy is a primary outcome of controlled force application.
Tooling Wear
Excessive stress on the forming rings leads to rapid degradation of the polished surfaces. Controlling the wall ironing pressure extends the interval between maintenance cycles and reduces the downtime of the stamping line.