Meaning
Hazardous self-sustaining exothermic reactions initiated inside a lithium ion cell during high current charging result from severe internal short circuits or violent degradation of over-lithiated cathode materials. Rapid lithium plating on the anode surface during aggressive charge rates creates metallic dendrites that penetrate the microporous separator. Fast charge thermal runaway occurs when local heating from high current density triggers solid electrolyte interphase decomposition before passive heat dissolution can cool the cell core.
This hazard condition terminates cell function and defines the upper operational boundary for fast charging protocols.
Plating Mechanism
Mass transport limitations in liquid electrolytes at high C-rates force the anode potential below zero volts against metallic lithium. Metallic lithium then deposits directly onto electrode surfaces instead of intercalating cleanly into the host lattice. These dendritic growths breach separator walls to establish direct electrical contact between opposing current collectors.
Heat Generation
Ohmic heating from localized short circuits accelerates exothermic chemical breakdown between active materials and organic solvents. Gas generation builds internal cell pressure until mechanical safety vents rupture.
Safety Threshold
Temperature monitoring at the cell terminal provides early detection of internal heat generation before uncontrolled self-heating begins. Current interrupt devices and thermal cutoffs disengage the charging circuit when voltage response curves indicate severe polarization.