Quantifying Environmental Stress Factors during Marine Cell Freight

Marine cell freight degrades inventory through thermal acceleration, terminal oxidation, and micro-motion fatigue; mitigate via under-deck DAP terms.

09.10.26 18 min

Hold

Electronic enclosures and a cylindrical battery cell rest on gravel against steel railway tracks alongside a blank memo card.

Thermal Stratification inside Ocean Containers

Container ships carry standard forty-foot high-cube containers in stacks up to nine tiers deep below deck and nine tiers high on weather decks. In an unventilated steel dry-van container, the internal microclimate is driven by marine air, direct solar exposure on upper tiers, and radiant heat from engine bulkheads or fuel-oil settling tanks. The air boundary layer beneath an exposed roof reaches equilibrium temperatures twenty to thirty degrees Celsius above ambient on tropical runs.

When transiting the Malacca Strait or the Red Sea in summer, ambient dry-bulb readings of thirty-five degrees Celsius routinely push air in topmost container tiers to fifty-five or sixty degrees Celsius.

Temperatures inside the box are far from uniform. Core pallets in dense blocks warm and cool sluggishly because of their thermal mass, but boundary packaging directly against side walls and ceilings follows the external diurnal solar cycle within ninety minutes. That temperature spread across a single pallet creates uneven electrochemical aging across otherwise identical production lots.

A container roof exposed to equatorial irradiance reaches sixty-five degrees Celsius while bottom corner castings rest at thirty-two degrees Celsius against wet steel deck plates.

Lithium-ion cells packed for marine transit encounter a decidedly uneven thermal field. A pallet of twenty-one-thousand-seven-hundred cylindrical cells stowed directly beneath the container roof sits in continuous high heat that accelerates parasitic chemical reactions. Pallets resting on the bottom floor over ballast tanks stay much cooler with minimal diurnal swings.

As a result, identical cells from the same production batch arrive at destination in divergent electrochemical states.

A composite battery separator material sample secured by a metallic clamping band hangs vertically within a dark industrial production testing facility.

Electrochemical Aging Rates under Sustained Heat

Thermal stress accelerates calendar aging through the Arrhenius relation, where reaction velocity roughly doubles for every ten-degree rise in temperature. In nickel-manganese-cobalt lithium-ion chemistries, sustained heat speeds up electrolyte decomposition and the progressive growth of the solid electrolyte interphase on the graphite anode, consuming cyclable lithium inventory. At higher states of charge, cathode transition metals dissolve, and free manganese and nickel ions migrate across the separator to poison the negative electrode.

Over a thirty to forty-five days passage through tropical shipping lanes at sustained temperatures between forty-five and fifty-five degrees Celsius, calendar capacity fade accelerates substantially compared to baseline warehouse storage at twenty degrees Celsius. Degradation follows square-root-of-time kinetics through this initial marine transit window, which tends to mask the onset of deeper degradation paths. Upon arrival, the increased resistance of the solid electrolyte interphase manifests as elevated direct-current internal resistance.

State of charge during transit directly dictates the kinetic barrier. Cells stored at fifty percent state of charge undergo higher anode potential stress and elevated side-reaction rates compared to those shipped at thirty percent state of charge. While International Civil Aviation Organization rules restrict international air freight of lithium-ion cells to thirty percent state of charge, ocean freight under the International Maritime Dangerous Goods Code carries no statutory thirty-percent ceiling, leaving state-of-charge limits to commercial agreement between shipper and consignee.

Buyers who permit cell suppliers to ship at fifty or sixty percent state of charge to satisfy domestic test protocols find substantial capacity loss on receipt. Cells resting in forty-eight-degree hold environments lose between one and two percent of nominal rated capacity across a standard four-week maritime passage. The impedance rise creates severe cell-to-cell capacity variance across the lot, preventing high-yield series string matching on subsequent pack assembly lines.

Swell

A steel industrial shredder assembly features a mounted ventilation duct and electrical power switch situated before a heavy duty metal crushing chamber.

Format-Specific Hermetic Integrity and Vapor Pressure

Atmospheric pressure drops with passing weather systems, while container interiors experience daily pressure swings tied to diurnal temperature cycling. The vapor pressure of volatile non-aqueous electrolyte solvents ~ particularly linear carbonates like dimethyl carbonate and ethyl methyl carbonate ~ rises exponentially with core cell temperature. Dimethyl carbonate exhibits a boiling point of ninety degrees Celsius at sea level, but even at fifty-five degrees Celsius its partial vapor pressure exerts significant continuous outward force against cell enclosures.

Cylindrical cells resist internal vapor expansion with rigid drawn steel cans with wall thicknesses ranging from zero point one five to zero point two five millimeters. The terminal header incorporates a current interrupt device and a mechanical rupture vent designed to open only between one point zero and one point eight megapascals. Prismatic cells employ deep-drawn aluminum cans with wall thicknesses between zero point six and one point zero millimeter, relying on laser-welded top covers and precision rupture foils engineered to relieve pressure around zero point eight megapascals.

Mechanical Boundary Characteristics by Cell Format Under Marine Cargo Stresses
Format Type Enclosure Material Wall Thickness (mm) Rupture Vent Threshold (MPa) Allowable Package Swell (mm)
Cylindrical 21700 Nickel-Plated Steel 0.18 ± 0.02 1.40 ± 0.15 0.05
Prismatic Large 3003 Aluminum 0.80 ± 0.05 0.75 ± 0.08 0.80
Pouch Medium Aluminum Laminated Film 0.12 ± 0.01 No Burst Disc 1.50

Pouch cells have no rigid external mechanical constraints. The enclosure consists of a flexible multi-layer aluminum laminated film sealed by a thermal bond layer of cast polypropylene typically forty to eighty micrometers thick. The cell volume expands directly in response to internal gas generation and elevated solvent vapor pressures.

Pouch cells shipped without mechanical clamping fixtures undergo continuous mechanical deformation across the seal periphery, concentrating shear stress along the tab feed-through seals where the positive aluminum and negative nickel or copper terminal tabs emerge.

A lithium ion pouch cell sits inside a black metal compression fixture equipped with a thermocouple and liquid electrolyte residue.

Mechanical Restraint during Waterborne Transit

Pouch cell geometry demands uniform external compression to maintain internal electrode layer alignment and prevent delamination of active material coatings from current collector foils. When unconstrained pouch cells encounter high temperatures, microscopic pockets of gas accumulate between anode and cathode faces. These gas bubbles displace liquid electrolyte, creating localized dry zones that permanently elevate ionic transport resistance.

Suppliers avoid shipping uncompressed pouch cells in loose nested plastic trays. Best packaging specifications mandate rigid foam inserts or structural shipping braces that maintain between twenty and fifty kilopascals of face pressure on pouch cell surfaces throughout transit. Prismatic cells packaged in high-density expander frames resist outward bulging of wide aluminum face walls.

Unconstrained prismatic cells exposed to thermal cycling exhibit permanent housing deflections exceeding zero point eight millimeters across their wide faces, preventing insertion into automated pack module carriers with tight mechanical clearance envelopes.

  1. Pouch face expansion breaks internal face contact and causes localized current crowding during initial formation cycling.
  2. Tab seal micro-cleavage introduces moisture into the cell interior, initiating hydrofluoric acid formation.
  3. Prismatic can deformation breaches module assembly dimensional tolerances, jamming automated cell placement equipment.
  4. Cylindrical gasket creep compromises the mechanical crimp, permitting gradual solvent evaporation into primary carton packaging.

The forwarder disclaims responsibility for enclosure distension once external packaging shows no physical crushing or liquid contamination.

Surge

A specialized testing apparatus holding a polymer membrane sample between two mechanical probes on a laboratory glass surface.

Vessel Dynamic Profiles and Ocean Motion Spectra

Commercial container vessels generate low-frequency continuous accelerations combined with stochastic impact shocks. The dynamic environment comprises six discrete degrees of freedom: translational heave, surge, and sway, alongside rotational roll, pitch, and yaw. Wave encounter frequencies during open-ocean passages generate sustained vertical heave and lateral roll accelerations between zero point one and zero point five hertz.

Large post-Panamax container vessels develop maximum roll angles exceeding twenty degrees in sea states six and seven. As the ship rolls, cargo secured in upper tiers far from the vessel roll center experiences substantial lateral acceleration components. These low-frequency cyclical forces operate continuously over weeks, inducing low-cycle mechanical fatigue across cell packaging systems, pallet strapping, and cell terminal pins.

Under sea state seven conditions lateral acceleration components at container deck tier seven reach zero point eight gravity units at zero point two hertz.

These motions differ fundamentally from the short-duration, high-acceleration shocks encountered during road transport or rough handling. Highway trucking generates transient impacts between two and ten gravity units with durations under twenty milliseconds. Marine transit subjects cells to millions of continuous stress reversals at low frequency, shifting mechanical loads across packaging partitions.

Loose individual cells slide against separator walls, creating micro-abrasion of exterior insulating jackets and degrading terminal insulator washers.

A heavy lithium battery module and metal enclosure are secured with straps on a cargo pallet inside an aircraft freight hold.

Vibration and Shock Boundaries across Shipping Methods

Mechanical verification testing under UN 38.3 standard covers transport safety qualification, but its vibration profiles do not replicate ocean freight dynamic profiles. Test T.3 of UN 38.3 applies a logarithmic frequency sweep from seven to two hundred hertz, completing one cycle every fifteen minutes for three hours per axis. This profile evaluates resonance behaviors typical of chassis vibration in road transport and turbo-prop aircraft freight, completely bypassing the continuous sub-hertz cyclic rolling loads that dominate marine passages.

Dynamic Stress Profile Comparison Between Maritime Transit and Regulatory Test Baselines
Stress Parameter Marine Transit Reality UN 38.3 Test T.3 UN 38.3 Test T.4
Dominant Frequency 0.1 Hz to 2.0 Hz 7.0 Hz to 200.0 Hz Transient Pulse
Sustained Acceleration 0.2g to 0.8g continuous 1.0g to 8.0g swept 150g peak (small cell)
Duration Per Axis 500 to 1,000 hours 3.0 hours Half-sine, 6 ms
Total Cycle Count 300,000 reversals ~ 36,000 cycles 18 total shocks

Because regulatory vibration protocols omit sustained sub-hertz excitation, cells pass mandatory compliance hurdles yet arrive with internal mechanical issues. Long-duration low-frequency cyclic shear weakens the ultrasonic or laser welds connecting electrode current collector tabs to terminal feed-through rivets. Pouch cell internal foil stacks, containing dozens of delicate copper and aluminum foils, undergo cyclic inertia displacement.

The unsupported ends of internal electrode flags tear at weld edges under repetitive lateral motion, creating latent short circuits that activate only during initial pack charging.

The standard freight forwarding liability clause caps transit damage recovery at two special drawing rights per kilogram of gross cargo weight unless higher values receive advance declaration on the bill of lading.

Rust

Cylindrical battery components form a vertical assembly supported by cylindrical cells resting on a horizontal metal plate beneath an industrial press.

Relative Humidity and the Cargo Sweat Mechanism

Ocean shipping routes traverse distinct marine climate zones, generating rapid shifts in ambient moisture levels. Relative humidity inside steel containers routinely hovers between seventy and ninety-five percent. Cargo loaded in warm, humid East Asian ports carries trapped ambient moisture inside the packaging materials, corrugated cardboard cartons, wooden pallets, and internal plastic separators.

Moisture release from hygroscopic packaging generates elevated relative humidity levels inside closed containers.

When the vessel crosses colder waters or encounters sudden temperature drops at night, the steel shell of the container cools faster than the cargo mass. As container skin temperature falls below the internal air dew point, condensation forms on the underside of the ceiling and along the upper walls. This phenomenon, termed cargo sweat or container rain, drips liquid water onto the topmost layer of cargo pallets.

Corrugated cardboard cartons soften upon absorbing moisture, losing structural compression strength and causing outer carton collapse under pallet stack loads.

An engineered structure undergoes dynamic testing, releasing a significant plume of fine airborne particles within a controlled dark space.

Electrolytic Corrosion of Exposed Terminals

Liquid moisture contact accelerates terminal corrosion. Cylindrical cells typically feature nickel-plated steel positive caps and cold-rolled steel negative can bottoms. Prismatic cells expose bare 1060 or 3003 aluminum positive terminals and nickel-plated copper or pure copper negative terminals.

Condensing water rich in marine chloride aerosols forms a highly conductive electrolytic film across exposed cell terminals.

Galvanic couples form between dissimilar metals in the presence of this moisture layer. At the negative terminal of a prismatic cell, copper and aluminum components establish substantial electrochemical potential differences. The resulting galvanic current drives localized pitting corrosion through protective nickel platings, creating non-conductive copper oxide and aluminum hydroxide crusts across terminal welding pads.

The formation of these oxidation layers prevents successful automated laser or ultrasonic wire bonding during module assembly, forcing lines into costly manual mechanical cleaning or total cell rejection.

  • Chloride ion deposition breaks down protective aluminum oxide passivating films, triggering rapid micro-pitting across terminal weld surfaces.
  • Corrosion product resistance introduces uneven interface impedances across parallel cell groups, unbalancing current distribution during operation.
  • Cardboard structural softening induces vertical stacking collapse, tilting interior cell layers and tearing fragile terminal isolation sleeves.

Condensation also compromises external polyimide or polyethylene terephthalate cell insulation wraps. Moisture wicking underneath the outer shrink-sleeve establishes conductive paths between the positive crimp rim and the bare steel can shoulder of cylindrical formats. This continuous microscopic leakage current drains cell state of charge during transit, causing low open-circuit voltage upon arrival that drops individual cells below critical chemical copper dissolution thresholds.

The buyer’s incoming inspection protocol discards cells showing open-circuit voltages below two point zero volts directly into hazardous waste processing.

Drift

Ruptured stainless steel thermal test enclosure rests on a metallic laboratory counter beside a small sample vial and stacked plates.

Degradation Kinetics across Thirty Transit Days

Cell capacity loss during ocean transit proceeds through distinct electrochemical pathways determined by environmental exposure. Take a concrete shipment of one hundred thousand lithium-ion cells: fifty thousand units of lithium iron phosphate chemistry and fifty thousand units of high-nickel nickel-manganese-cobalt chemistry, loaded into an ocean container transiting an equatorial route over thirty days. The mean container temperature averages forty degrees Celsius with peak daytime excursions touching fifty-five degrees Celsius.

The cells enter the container at thirty-five percent state of charge.

Capacity loss during pure calendar aging follows an empirical power law where fade equals a kinetic rate coefficient multiplied by time raised to an exponent near zero point five. The kinetic rate constant adheres to Arrhenius behavior, governed by an apparent activation energy of roughly fifty kilojoules per mole for lithium iron phosphate and sixty-five kilojoules per mole for high-nickel nickel-manganese-cobalt. At forty degrees Celsius, the kinetic constant accelerates by a factor of three point two for lithium iron phosphate and four point zero for nickel-manganese-cobalt relative to baseline warehouse holding at twenty degrees Celsius.

Lithium iron phosphate cells demonstrate robust stability, yielding nominal calendar capacity fade of zero point two percent across thirty days. High-nickel nickel-manganese-cobalt cells experience elevated side-reaction rates, losing approximately zero point six percent of initial rated capacity over the same period. The capacity loss concentrates cyclable lithium into parasitic solid electrolyte interphase species, locking that capacity away permanently.

A technician in blue protective workwear pours liquid from a container onto a lithium battery module inside an industrial testing laboratory.

Impedance Growth and Voltage Decay Profiles

Impedance growth creates greater operational disruption than bulk capacity loss. The growth of resistive films on negative electrode surfaces increases direct-current resistance. For high-nickel chemistries, thirty days at an average temperature of forty degrees Celsius elevates direct-current internal resistance by six to ten percent.

In extreme boundary positions near the container ceiling, where local average temperatures reach fifty degrees Celsius, resistance jumps by fifteen to twenty-two percent.

Open-circuit voltage drops as parasitic current draws deplete electrode charges. A lithium iron phosphate cell operates on an exceptionally flat voltage plateau between twenty and eighty percent state of charge. A voltage drop of five millivolts corresponds to a significant state-of-charge shift across that plateau.

Nickel-manganese-cobalt cells display a steeper voltage slope, allowing more direct tracking of state-of-charge drift from voltage measurements.

The variance of these degradation metrics matters more than the mean. Because container temperatures vary by fifteen to twenty degrees Celsius from core to perimeter, identical cells develop a broad, bimodal performance distribution upon destination arrival. A batch entering transit with a tight open-circuit voltage spread of two millivolts arrives with a spread of twenty-eight millivolts, destroying sorting and grading uniformity established at the factory formation line.

Detecting this latent transit damage requires specific screening methods before cells reach automated module welding lines.

Audit

A reinforced protective glove strapped to a concrete impact plate stands mounted on steel structural columns inside a heavy manufacturing assembly plant.

Dockside Inspection Sequence and Sampling Plans

Evaluating cell shipments immediately upon container unstuffing prevents degraded stock from entering storage or automated assembly lines. The incoming verification protocol operates on an ANSI/ASQ Z1.4 normal inspection sampling plan at General Inspection Level II, selecting an Acceptance Quality Limit of zero point four percent for major functional defects and one point zero percent for minor cosmetic non-conformances. The receiver pulls sample units systematically from three container zones: container top ceiling layer, container core center, and bottom floor corners.

  1. Verify tamper-evident container door seals and download primary transit datalogger records, cross-referencing shock events, relative humidity traces, and sustained temperature profiles against shipping specifications.
  2. Inspect exterior master cartons across all pallet layers, recording any carton crushing, structural softening, mold presence, or watermark stains from container condensation.
  3. Examine cell exterior packaging units, verifying desiccants inside sealed moisture-barrier bags have not reached moisture saturation thresholds.
  4. Inspect individual cell enclosures, screening for housing bulge, insulator sleeve pinholes, tab micro-cracking, and corrosion deposits on positive or negative contact faces.
  5. Measure rest open-circuit voltage and alternating-current internal resistance at one kilohertz using a four-wire Kelvin test fixture under temperature-controlled cleanroom conditions at twenty-five degrees Celsius.
  6. Subject a secondary sample subset to direct-current internal resistance testing via hybrid pulse power characterization to detect early solid electrolyte interphase thickening.

This verification flow isolates mechanically or chemically damaged lots before unpacking costs accumulate. Rejection occurs immediately if environmental loggers record temperatures exceeding fifty-five degrees Celsius for longer than forty-eight continuous hours, or if shock loggers register single impact events exceeding three gravity units across any translation axis.

A heavy steel wire mesh container descends toward an angled polymer transport crate secured on a mechanical test fixture.

Voltage and Resistance Acceptance Thresholds

Electrical testing weeds out cells damaged by parasitic chemical discharge or internal micro-shorts. The test engineer measures open-circuit voltage to a precision of zero point one millivolt using a calibrated six-and-a-half-digit digital multimeter, comparing the values against factory shipping manifest inspection reports.

A nickel-manganese-cobalt cell leaving the factory at three point six five zero volts must land within a tight voltage band. If open-circuit voltage falls below three point六二零 volts, or if the distribution spread across the inspected sample exceeds fifteen millivolts, the lot is quarantined. Alternating-current internal resistance measured at one kilohertz flags contact interface degradation.

An impedance shift exceeding ten percent above factory pre-shipment values points to moisture-induced terminal oxidation or internal collector tab weld failure.

A measured shift in one-kilohertz AC impedance exceeding twelve percent above factory pre-shipment values mandates immediate quarantine of the entire pallet batch.

While module balancing and initial conditioning cycles can compensate for minor impedance differences, severe maritime degradation leaves permanent capacity variation across series strings.

Cargo

A coin cell battery rests on the fabric placket of a white dress shirt beside warehouse logistics motion trails and industrial material handling equipment.

Packaging Architectures and Desiccant Load Arithmetic

Controlling the container microclimate requires purpose-built packaging at every level. Standard single-wall corrugated board softens quickly under marine conditions. Battery freight relies on heavy-duty double-wall or triple-wall corrugated cartons treated with external hydrophobic coatings, combined with internal antistatic vacuum-sealed aluminum-foil moisture barrier bags.

Desiccant sizing uses established packaging standards such as DIN 55474 or MIL-D-3464E. Desiccant requirements depend on container volume, interior hygroscopic packing weight, water vapor transmission rates of barrier films, and expected transit duration. One standard desiccant unit corresponds to the adsorption capacity for six grams of water vapor at forty percent relative humidity at twenty-five degrees Celsius.

Calculating the exact desiccant charge prevents condensation inside barrier packaging.

Assume an export pallet carrying five hundred kilograms of cells packed with twenty kilograms of corrugated internal dividers and five kilograms of polyethylene protective foam. The pallet is enclosed within a high-barrier aluminum laminate bag with a surface area of six square meters and a verified water vapor transmission rate of zero point zero five grams per square meter per day. For a transit duration of forty-five days under tropical conditions, the mass of water vapor permeating the barrier envelope equals thirteen point five grams.

The internal hygroscopic cardboard and foam, loaded at an initial equilibrium moisture content of eight percent by weight, releases up to four hundred grams of water vapor inside the sealed volume as temperature increases.

The total moisture burden approaches four hundred and fourteen grams of water. Dividing this mass by the six-gram capacity of a standard desiccant unit yields an absolute minimum requirement of sixty-nine desiccant units per pallet. Placing seventy-five desiccant units inside the moisture barrier bag guarantees relative humidity remains under thirty percent throughout the forty-five-day marine passage.

Parallel high voltage composite cables rest upon rigid industrial support brackets extending down a long testing tunnel.

Contractual Boundaries and Freight Responsibility

Mitigating maritime risk requires aligning commercial shipping terms with technical packaging controls. The selection of Incoterms defines where transfer of risk and physical custody occurs. Under Free On Board terms, risk transfers to the buyer the moment goods cross the vessel rail at the export port, leaving the buyer exposed to all marine transit risks.

Specifying Delivered at Place terms shifts the risk of maritime degradation onto the cell manufacturer until the shipping container arrives at the buyer destination facility. When negotiating cell supply contracts, technical annexes should enforce specific maritime protective clauses. The technical agreement must mandate reefer container transport set to fifteen degrees Celsius for high-nickel cathode formulations, precluding high heat exposure.

Where the cost of refrigerated reefer containers proves prohibitive for low-margin projects, shipping agreements should require stowage under deck away from heat sources. Under-deck stowage prevents direct solar loading and insulates cargo from external diurnal temperature swings, maintaining cargo temperatures within five degrees Celsius of ambient sea surface water.

Contractual agreements must stipulate that open-circuit voltage drift exceeding twelve millivolts or impedance increases exceeding eight percent from factory departure levels constitute arrival non-conformances. Defining objective electrical parameters within the purchase contract transfers the cost of marine stress factors back to the supplier, ensuring careful container selection and robust packaging long before freight clears the export terminal.

Nomenclature

Solid Electrolyte

Meaning ~ Solid-state materials that conduct lithium ions replace the traditional liquid electrolytes used in conventional batteries.

Open Circuit Voltage Drift

Meaning ~ Gradual change in the measured electrical potential of an disconnected battery cell over a specific storage period indicates internal self-discharge or chemical instability.

Arrhenius Equation

Meaning ~ Mathematical formulas describe chemical reaction rates as an exponential function of absolute temperature and activation energy.

UN 38.3

Meaning ~ A mandatory United Nations testing standard outlines safety requirements for the transport of lithium metal and lithium-ion batteries.

Hybrid Pulse Power Characterization

Meaning ~ Voltage response measurement determines the resistance and capacity characteristics of energy storage cells under transient load conditions.

Dimethyl Carbonate

Meaning ~ A flammable organic liquid with a mild odor, dimethyl carbonate acts as a versatile chemical intermediate and a polar solvent in lithium-ion battery electrolyte formulations.

Non Aqueous Electrolyte

Meaning ~ Liquid formulations lacking water function as a non aqueous electrolyte within lithium ion cells to transport lithium ions between electrodes during charge and discharge cycles.

Current Interrupt Device

Meaning ~ Mechanical safety component integrated into the header of a cylindrical cell disconnects the electrical path during an overpressure event.

Tab Micro-Cleavage

Meaning ~ A specific mechanical defect occurs when the metallic current collector foil within a lithium-ion cell develops microscopic fractures or separations at the junction point where the tab attaches to the electrode sheet.

Electrolyte Decomposition

Meaning ~ The chemical breakdown of the liquid organic compounds within a battery occurs when voltages or temperatures exceed the stability window of the components.

Internal Resistance

Meaning ~ Total opposition to electrical current flow within an operating cell generates instantaneous ohmic voltage drops and operational thermal dissipation.

Incoterms

Meaning ~ Universal set of three letter trade definitions establishes the rights and obligations of buyers and sellers in international sales contracts.

What the firm knows, published

Expertise is a utility, not a secret. sentiention™ publishes its working knowledge as open reference: intelligence layer covering the materials it sources, the markets it enters, and the reference that serves both.