Modeling Radial Solid Electrolyte Interphase Thickness in Fast-Charged Cylindrical Cells
Fast-charge radial SEI thickening concentrates at the cylindrical core due to anisotropic thermal resistance, demanding core cooling to prevent premature fade.

Gradient
Heat dissipation in spirally wound lithium-ion cells follows an anisotropic path dictated by material layers. The alternating stack of active coatings, copper foil, aluminum foil, and polymeric separators sets up a severe directional disparity: axial thermal conductivity along the current collector foils reaches 20 to 30 Watts per meter-Kelvin, while radial conductivity across the laminate layers remains trapped between 0.15 and 0.85 Watts per meter-Kelvin. When forced convective cooling is applied only to the outer can during a 3C constant-current charge, heat must escape across that low-conductivity winding thickness, inevitably pooling at the geometric core of the jelly roll.
Each charging step drives coupled electrochemical reactions with rates tied to local operating temperatures. Under Arrhenius kinetics, parasitic electrolyte reduction accelerates sharply wherever internal temperatures peak, and at an ambient baseline of 25 degrees Celsius, large-format cylindrical cells without direct internal cooling quickly develop core-to-surface gradients of 10 to 22 Kelvin. Because liquid electrolyte conductivity, solid-state graphite diffusion, and charge-transfer rates all climb with temperature, the warmer inner windings exhibit lower total internal impedance than the cooler perimeter.
Current shifts inward as a result, concentrating heavily in the core during the opening stages of high-rate charging.
Continuous 4C charging at 25 degrees Celsius ambient generates a radial temperature differential exceeding 18 Kelvin in uncooled 4680 mandrels.
In jelly rolls relying on single-tab layouts at terminal ends, current collection sets up axial and circumferential gradients that worsen the underlying radial thermal spread. Continuous tabless and multi-tab architectures eliminate much of the ohmic heating at collector foil joints, which leaves radial conduction across separators and coatings as the primary thermal bottleneck. This persistent divergence in current density forces anode overpotentials to drift unevenly against lithium reference potentials from wrap to wrap.
| Format Specification | Radial Conductance (W/m-K) | Radial Delta T at 80% SOC (K) | Core Current Density Ratio | Outer Wrap Current Density Ratio |
|---|---|---|---|---|
| 18650 Cylindrical (2.5 Ah NMC811) | 0.72 | 4.8 | 1.08 | 0.94 |
| 21700 Cylindrical (5.0 Ah NMC811) | 0.58 | 9.6 | 1.17 | 0.89 |
| 46800 Tabless (24.0 Ah NMC811) | 0.31 | 19.4 | 1.34 | 0.78 |
| 46950 Tabless (30.0 Ah NMC811) | 0.28 | 23.2 | 1.41 | 0.72 |
External can-cooling systems are routinely specified to hold the exterior steel case below 35 degrees Celsius throughout charging, but keeping the container cool does not resolve the non-uniform degradation running through the internal windings.

Flux
Mass transport across the interphase film involves neutral solvent molecules diffusing through an inorganic and organic boundary layer toward the electrochemically active graphite surface. Below 0.8 Volts relative to pure lithium, ethylene carbonate and linear alkyl carbonates accept electrons to form insoluble reduction products ~ chiefly lithium carbonate, lithium alkyl carbonates, and lithium fluoride ~ along with gaseous byproducts. Because electron tunneling drops off exponentially beyond two nanometers from the substrate, passivating growth across hundreds of cycles is sustained solely by the physical transport of solvent through porous outer deposits.

Coupled Electrochemical Continuum Formulations
Modeling radial passivation requires coupling Newman-style porous electrode theory with energy conservation and solvent transport equations. The flux of neutral solvent reaching the negative electrode interface couples directly to cathodic side-reaction current densities across several interdependent physical domains:
- Solvent Concentration Profile describes reactant density throughout the porous passivating deposit, solved through Fickian diffusion using a temperature-dependent diffusion coefficient.
- Parasitic Current Density tracks the consumption rate of cyclable lithium inventory via cathodic Tafel kinetics linked to local mixed potential and protective film resistance.
- Thermal Energy Conservation balances heat generated by reaction overpotentials, entropic shifts, and Joule heating across the radial coordinate of the jelly roll.
- Film Resistance Accumulation evaluates the progressive ohmic drop across the interface as insoluble decomposition products accumulate cycle by cycle.
Where elevated local current density meets cooler peripheral turns, graphite particle potential relative to the adjacent liquid electrolyte frequently slips below zero Volts. That crossover triggers metallic lithium plating alongside normal solvent reduction. The plated metal then reacts directly with incoming solvent, laying down secondary interphase films marked by high porosity and poor mechanical cohesion.

What Drives Radial Overpotential Imbalance during Charging?
Radial disparities in local overpotential stem from non-linear feedback between temperature-dependent electrolyte transport and current distribution. In the hot core, higher liquid-phase ionic conductivity suppresses liquid-junction polarization, and faster solid-state diffusion accelerates lithium intercalation into the graphite host. Near the colder exterior casing, however, sluggish liquid-phase transport drives the intercalation overpotential significantly more negative, leaving outer wraps vulnerable to lithium plating during constant-current charging.
Passivating film growth consumes both cyclable lithium and free solvent. High-energy cylindrical designs rarely carry more than 3.5 grams per ampere-hour of liquid electrolyte to begin with, so preferential solvent consumption at the core brings about localized dry-out long before the cell exterior starves. As that surface film thickens, compounding contact resistance from winding tension, its rising ionic resistance throttles lithium-ion flux during discharge, driving up cell impedance unevenly across the spiral winding.
Electrolyte decomposition accelerates along the inner winding where heat dissipation reaches its geometric minimum.
It remains unsettled whether long-term film growth under fast charging is primarily limited by neutral solvent diffusion through developing nanopores or by radical cation migration through the dense inorganic base layer.

Core
Centerpin regions endure the sharpest mechanical loads in a cylindrical cell. During assembly, the winding mandrel applies tension to the foil collectors to seat the separator and prevent electrode slippage during downstream handling. Once that mandrel is extracted, the innermost wraps retain severe hoop stress, compressing the porous active coatings and choking off tortuous paths needed for electrolyte transport.

Why Do Inner Mandrel Layers Degrade Faster?
Bending curvature peaks sharply against small-diameter center cavities. In standard 18650 and 21700 cells, inner radii run between 1.5 and 2.5 millimeters, subjecting coated electrodes to severe mechanical flexure. This forces micro-delamination between the graphite layer and the copper foil on the inner face while stretching the outer face under tension.
As charging heats the mandrel zone, accelerated side reactions precipitate decomposition products inside these micro-fractures, prying active particles apart.
| Radial Position (r / R_max) | SEI Thickness (nm) | Active Layer Porosity (%) | Capacity Retention (%) | Film Resistance (Ohm-cm2) |
|---|---|---|---|---|
| 0.08 (Innermost turn) | 142.5 | 18.2 | 68.4 | 48.6 |
| 0.25 (Mid-core) | 118.0 | 21.5 | 74.1 | 37.2 |
| 0.50 (Mid-radius) | 84.2 | 26.0 | 82.6 | 22.4 |
| 0.75 (Outer-mid) | 56.1 | 28.4 | 89.3 | 14.8 |
| 0.98 (Outermost turn) | 42.7 | 30.1 | 93.5 | 11.2 |
Rigid boundary constraints force expanding surface films into surrounding porous media. As passivation thickens on the inner graphite wraps, it pinches the sub-micron pore networks of adjacent separators; polypropylene and polyethylene membranes drop from nominal 40 percent porosities to under 20 percent through localized compressive creep. Degradation through the jelly roll unfolds in a clear sequence:
- Core heat accumulation accelerates solvent reduction during high-rate charging.
- Solid decomposition products clog electrode void space, restricting ionic conduction.
- Radial expansion against the centerpin boundary promotes delamination between current collectors and active coatings.
- Salt depletion starves internal wraps, shifting local potentials into regimes that induce metallic lithium deposition.
- Asymmetric mechanical expansion distorts the jelly roll, inducing wrap buckling and early capacity cutoffs.
Jelly-roll wraps nearest the center pin consume available salt before outer wraps reach operating temperature.
If pack design ignores this concentration of degradation at the mandrel, battery systems can suffer sudden capacity drops in the field, driving warranty claims and unexpected pack retirements.

Audit
Qualifying cylindrical cells for commercial fast-charging duty requires destructive physical teardowns alongside routine cycling tests. Single-channel potentiostat testing hides radial variance because terminal voltage readings aggregate the response across all parallel windings. Resolving actual spatial gradients in interphase growth requires post-mortem electrode harvesting inside an argon glovebox held below 0.1 parts per million oxygen and moisture.

Physical Cross Section Metrology and Spectroscopic Validation
Opening cycled cells without destroying delicate organic interfaces requires circumferentially slitting the nickel-plated steel can before carefully unrolling the jelly roll. Each turn is logged from the perimeter to the core, and electrode coupons extracted across the radius are subjected to targeted characterization:
- Cryogenic Focused Ion Beam cross-sectioning preserves soft organic deposits against ion-beam heating to image local thickness variations on active particles.
- X-Ray Photoelectron Spectroscopy depth profiling quantifies shifting ratios of dense inorganic lithium fluoride to porous organic polycarbonates wrap by wrap.
- Electrochemical Impedance Spectroscopy on symmetric coin cells reassembled from harvested strips isolates film resistance from charge-transfer resistance for each radial zone.
- Inductively Coupled Plasma optical emission spectrometry determines lost cyclable lithium inventory by measuring immobilized lithium and transition metal deposition on harvested anodes.
Cryogenic cross-sections show that isothermal electrochemical models underestimate core interphase growth by 30 to 65 percent. Treating thermal parameters as uniform across the winding overlooks the heat trapped by low transverse conductivity. Accurate lifetime models must dynamically couple the solid electrolyte diffusion coefficient to both local compressive stress and real-time radial temperature.
IEC 62660-1 capacity retention guarantees fail early whenever cycle profiles disregard thermal variance between electrode turns.
Supply contracts referencing standard IEC 61960 capacity checks without mandating teardown verification of internal film thickness leave buyers exposed to unexpected impedance rise and premature warranty claims.

Settlement
Commercial exposure to fast-charge degradation settles squarely on warranty reserves and delivered energy cost per dollar of procured cell capacity. Buying cylindrical cells strictly against nominal C-rate datasheets prices the product on the assumption of uniform aging. Under fast-charge duty, radial film divergence accelerates until choked transport and capacity loss in the innermost turns end the practical life of the pack, regardless of how much active capacity remains in outer wraps.
| Cooling Configuration | Cell Cost ($/kWh) | Thermal Hardware ($/kWh) | Cycles to 80% Retention (3C) | Delivered Energy Cost ($/kWh-cycle) | Warranty Reserve Ratio (%) |
|---|---|---|---|---|---|
| Can Surface Only (Radial Dissipation) | 84.00 | 12.50 | 450 | 0.214 | 14.5 |
| Dual Surface and Tab Cooling | 84.00 | 21.00 | 820 | 0.128 | 6.2 |
| Internal Mandrel Core Cooling | 96.00 | 28.50 | 1,450 | 0.085 | 2.8 |
| Uncontrolled Ambient Convection | 84.00 | 4.00 | 280 | 0.314 | 26.0 |
Thermal management spending functions as a hedge against field warranty claims, yet cooling plates that contact only the outer cans of 4680 or 4695 cells deliver poor economic return over long operating cycles. Core degradation continues inside despite surface chilling; as the inner turns exhaust cyclable lithium, module impedance climbs until battery management systems trip premature low-voltage cutoffs under dynamic load.
Long-term cell supply agreements require grading and acceptance criteria tied to localized degradation thresholds rather than gross retained capacity alone. Without destructive teardown audits of core passivation thickness following accelerated fast-charge burn-in, integrator organizations absorb degradation risks that datasheets conceal. True cell longevity tracks the temperature of the innermost wrap, no matter how cold the casing is kept.